Read everything about the acquisition of Quantachrome by Anton Paar here

High Pressure Gas Sorption-
Characterizaton of Sorbent Materials

iSorb HP1 | HP2 -
High Pressure Gas Sorption Analyzer

PERFORMANCE iSorb HP1 iSorb HP2
Analysis stations 1 2
Gas input 2 (optional 4) 2 (optional 4)
Max pressure data (absolute) 100 or 200 bara 100 or 200 bara
Min pressure data 0.0005 bar 0.0005 bar
LP transducers 2 (1 bar) 3 (1 bar)
HP transducers 2 3
Total transducer count 4 6
Tranducer accuracy <±0.05% f.s. <±0.05% f.s.
Vacuum pump internal internal
Turbo pump option yes yes
Degas type automatic automatic
Degas ports in-situ in-situ
Max degas temp ( oC ) 500 500
Cryo option yes yes
Thermostatted bath (option) yes yes
Booster option yes yes
Thermostatted manifold yes yes
Gas inputs/vents location Side, for easy access Side, for easy access

a or 100 bar for lower pressure model.

PHYSICAL iSorb HP1 iSorb HP2
Height 100 cm (39.25in) 100 cm (39.25in)
Width 85cm (33.5 in) 85cm (33.5 in)
Depth 50.5 cm (19.25 in) 50.5 cm (19.25 in)
Weight 150 kg (330 lbs) 150 kg (330 lbs)

 

iSorb HP