Poremaster Mercury Intrusioin Porosimeters

Transducer
Pressure Range
PoreMaster 60 PoreMaster 33
0 - 50 psia*
     § Accuracy:
      Resolution:
950 - 4.26 µm dia.
± 0.11 % fso**
0.000763 psia
950 - 4.26 µm dia.
± 0.11 % fso
0.000763 psia
0 - 1500 psia
     § Accuracy:
      Resolution:
10.66 - 0.142 µm dia.
± 0.11 % fso
0.0229 psia
10.66 - 0.142 µm dia.(Upgrade)
± 0.11 % fso
0.0229 psia
0 - Maximum psia
     § Non-linearity:
       § Hysteresis:
          Resolution:
10.66 - 0.0036 µm dia.
± 0.05 % fso
± 0.10 % fso
0.916 psia
10.66 - 0.0064 µm dia.
± 0.05 % fso
± 0.10 % fso
0.511 psia
*Pounds per Square Inch Absolute ** Full Scale Output § Manufacturer's Specifications
Sample Cells
Sample Volume Intrusion Capacity Volume Resolution
3.2 cc 2.0 cc 9x10-5 cc
3.2 cc 0.5 cc 3x10-5 cc
6.6 cc 2.0 cc 9x10-5 cc
6.6 cc 0.5 cc 3x10-5 cc
18.0 cc 2.0 cc 9x10-5 cc
18.0 cc 0.5 cc 3x10-5 cc
Physical
Width: 20.25 in. 51.44 cm
Depth: 25.50 in. 64.77 cm
Height: 30.75 in. 78.11 cm
Weight: 398 lbs. 179 kg
Electrical
Mains: 100 - 240 volts AC, 50 Hz/60 Hz
Power: 1000 VA
Required